Ken, I was referring to the support pins used to support the panel from the underside in the placement machine. If one's misplaced or the wrong length, you can get a repeatable, very localized component defect. Bruce -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist Sent: Monday, April 28, 2008 4:32 PM To: [log in to unmask] Subject: Re: [TN] Cracking Ceramic Cap Here are some answers to your questions: Dave, [is there an end cap metallization such as nickel or copper between the solderable surface finish and the ceramic metalized layer?] I'm not sure. I've asked Steve to post one more picture of the end of the fractured cap. Mike, [Is your selective pallet hitting the cap in question when you load/unload the board?] Nope, I've checked the pallets and they are good with plenty of clearance. Werner, [The problem with Pb-free soldering is that all your caps... My recommendation is to reduce all cap pads, and RRs as well, to half the cap widths to reduce the size of the solder fillet 'vise grips.' Those pad widths were needed for wave soldering and the fillets for inspection.] We are using SN63 not that other stuff ;-) We are a EMS so have very little control over our customer but will certainly share your comments with them. Any thoughts on an intermediate fix? What do you mean by "... RRs as well"? Bruce, [Possible support pin placement issue?] I'm not sure what you mean by "possible support pin placement issue". I'm guessing you are saying the same thing as Werner though. Thank you, KennyB --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------