Ryan, I've seen PTH cracks in the past & I'd bow to the superior knowledge on the root cause already expressed on the matter. My own experiences of this problem is that its a time consuming & frustrating problem to diagnose & guarantee a fix, so I apply a series of design rules when laying out a PCB that tries to build in some fail safes (may not suit everyone but these work for me) in case the PCB fab is having an off day so my two cent's - - Hole Aspect ration ¡Ü6:1 - Copper wall thickness 30um Minimum - Inner layer redundant pad's must be retained - Annular ring of the inner layer pads to be 0,30mm (Drill + 0,60mm) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------