Well written, Terry! General areas of a board is seldom a contamination problem, but ENTRAPMENTS, yes! And one can not be sure the ionic contamination test tells you about them. /Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry L. Munson Sent: den 18 april 2008 22:35 To: [log in to unmask] Subject: Re: [TN] Ionic Contamination Question (& added info). Bill As one of the active task group participants during the 90s when we were asked to update the equivalence factors table and using low solids cleanable and no clean formulations, we found it difficult to assess these new types of low solids residues and if you look at the large detailed report from the task group (IPC TR 583) we found it difficult to correlate between static and dynamic systems. The use of higher pass fail criteria were in place for automotive users (one in particular used 28 ug/in2 instead of the 14 ug/in2 from 1978 to 1991 with no field performance problems related to flux residues with mean levels at 21 ug/in2 while using an 18-24% solids RMA flux) that did not see problems. My concern with cleanliness is not the generalized cleanliness of a total board but the amount of contamination present between pads, in via's or thru-hole devices. The pocket of contamination below an 0805 capacitor has created drained batteries when the entire assembly tests clean by ROSE and by bag extraction Ion Chromatography. It is only when we look at the localized pocket of contamination do we see the direct correlation to field and reliability performance. Many of the localized areas we look at with the C3 tester are clean and show low levels of contamination, but when we see the combined processing effects of selective wave soldering using a pallet to isolate the area we find that the residues that can be trapped between the pallet and circuit board (low solids no clean VOC free) are also protected from the heat but are very corrosive due to the water carrier and acidic pH 2.35. Dendrites are growing in these nearby areas, as well as stray voltage problems and intermittent performance issues and No Trouble Found (NTF) returns. It is important to understand the cleanliness of an assembly but it is more important to understand the cleanliness of the processing steps such as 1st reflow, 2nd reflow, wave soldering bottom and top side, bare board unsoldered areas, micro via's that have fabrication residues trapped inside causing performance problems and the hand solder / touch up residues. This type of cleanliness understanding comes from being able to do localized non-destructive residue assessment and ion chromatography analysis. Cleanliness testing must predict field performance. Using localized testing is the only way I am aware of understanding how much contamination is present in the areas of critical circuitry that tends to fail earliest. Terry Munson Foresite 765-457-8095 _www.Residues.com_ (http://www.Residues.com) In a message dated 4/18/2008 1:54:54 P.M. Eastern Daylight Time, [log in to unmask] writes: As perhaps the only person still around that attended the meetings resulting in the equivalence factors and IPC Cleaning & Contamination Chair at that time, perhaps a few points would facilitate the discussion: 1. The Navy set up the ionic testing development program to solve a serious failure problem in S.E. Asia. It worked. 2. In the timeframe when the test was developed and put in place by the military, most of the rest of the electronics industry in the US used the mil specs since they were free. 3. As the IPC set up and adopted Classes 1-3 (basically toys up to military/high rel), I asked the committee if we used the mil test result for Class 3, could we use 1.5x that limit for Class 2 and 2-3x for Class 1? The response was that with proper cleaning, the mil limit could readily be achieved while serving to monitor daily production. So the industry continued to use the (free) mil spec test standard. 4. The ionic contamination test was a valuable monitoring tool, since the SIR tests were done on coupons, not on actual assemblies, and took 1-2 weeks to complete. Needless to say, a high volume electronics producer could turn out a significant volume of PWAs during that time, often shipping them into the field as soon as assembly was completed. 5. As noted in my SMT column (offered yesterday) T. O. Duyck of Northern Telecom was charged with implementing water soluble flux for NT electronics production. During that time he observed and reported the differences in flux residue release rates, pointing out that rosin ca 90% of rosin flux residues release from the PWA surface during the 10-15 test time for ionic test equipment, while water soluble flux residues may take up to 2 hrs. to achieve the same level of release. Thus the release rate should be checked to ensure the flux used, time test time and the instrument employed provide reliable results and guidance to the production engineer. (See T. O. Duyck and M. Boulos, "Water Washes Reliability into Telephone Circuit Packs", IPC-TR-206, April, 1978) Based on this work, I investigated the release rate of SA flux residues, finding it even faster than rosin fluxes. (See W. G. Kenyon, "Synthetic Activated (SA) Flux Technology: Development, Commercialization, Benefits and Future Applications", Internepcon Japan, 24 Jan. 1986) 6. In the late 1980's, the materials and acceptance of the no clean or low residue or acceptable dirt concept became widely accepted and implemented on the designs of the time. Outsourcing to contract assemblers (both in the US and overseas) became widely practiced, so much of the former 'in-house' cleaning expertise disappeared. 7. This was seen at IPC as the number of company sponsored volunteers dwindled. Could we take on projects today to develop an updated ionic test for pr ocess monitoring? Find enough participants to conduct statistically sound round robin testing? Bill Kenyon Global Centre Consulting 3336 Birmingham Drive Fort Collins, CO 80526 Tel: 970.207.9586 Cell: 970.980.6373 **************Need a new ride? Check out the largest site for U.S. used car listings at AOL Autos. (http://autos.aol.com/used?NCID=aolcmp00300000002851) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- **************Need a new ride? Check out the largest site for U.S. used car listings at AOL Autos. (http://autos.aol.com/used?NCID=aolcmp00300000002851) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------