I would agree with Wayne. I would ask as well if you meant solder mask plugged or solder mask tented. If you cap both ends of a plated through hole with solder mask, it is not unusual to have the mask crack. Even a hairline crack can suck fluids in by capillary action. I have seen instances where residual sulfuric acid from a plating operation did just this, etching a circumferential area in the center of the hole, resulting in the kind of barrel cracking you describe. Wrote a magazine column on it. Doug Pauls Rockwell Collins "Thayer, Wayne" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 04/22/2008 04:51 PM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Thayer, Wayne" <[log in to unmask]> To [log in to unmask] cc Subject Re: [TN] Via barrel cracks I've never seen that. Usually the flux trapped in the partially sealed cavity can perform that function! -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ryan Grant Sent: Tuesday, April 22, 2008 5:45 PM To: [log in to unmask] Subject: Re: [TN] Via barrel cracks Hi Wayne, Understood. Can the solder mask solvents cause corrosion too? (Just checking everything...) Thanks, Ryan -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne Sent: Tuesday, April 22, 2008 3:42 PM To: [log in to unmask] Subject: Re: [TN] Via barrel cracks Hi Ryan! Werner gave a good rundown. I just wanted to question your comment about "plugged with solder mask from both sides". Solder mask is not designed for plugging at all. You need to specify a Pb-free compatible via plugging paste. Solder mask is loaded with solvent and rarely makes a decent "tent" over a via. Wayne Thayer -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ryan Grant Sent: Tuesday, April 22, 2008 1:43 PM To: [log in to unmask] Subject: [TN] Via barrel cracks Hi Technetters, I have a case of via barrel cracks (E crack) and I would like to know possible causes. The crack is circumferential and occurs at the center of the via. The hole appears smooth, i.e., no glass nodules or tearout and there is neither positive nor negative etchback. Of course there is some wicking, but only about 25um max. The copper thickness is 20um at the crack and roughly 35-40um at the knee. Although, at the initiation point of the crack, the copper thickness is only 10um, but that could be due to stretching and subsequent thinning of the copper. Around the periphery of the crack are micro-voids in the resin about 30um. It is triangular shaped, so I can't tell if it is resin recession or a laminate crack. In other words, this via pretty much looks normal, except for one thing, which might be an artifact of stretching and cracking of the via. For a span of about 60um on the vertical of the via, at the crack, there is a roughness that slightly reduces the copper thickness. The surface of the copper at this point appears both rough and black in color. This board has seen two reflows and a hot functional test before final failure. The board shop's initial response was speculation of the OSP soft etch attacking the copper, but this particular via has solder mask plugging both sides of the via; therefore chemicals after solder mask cure can not get into the via. In case it matters, at one time, we have had occurrences of this board shop "re-working" panels after copper plating by placing the panel in a tank of etchant, then re-running the board through copper plating. (They do panel plating). I'm a little suspicious of their FA, so I would like some independent opinions and places for me to dig into. Thanks for any help, Ryan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------