We tinposit bare copper milled PCBs to improve solderability. You can also very lightly scrub with a green pad to remove oxidation. The bottom line is bare copper solderabilty is poor compared to a finished PCB. In cases where you have no choose, RMA flux can improve your solderability on bare copper. I deal with the worst possible cases regularly. Shelf life depends on environment, storage condition, and laminate type. I have restored bare copper PCBs years old. Depending on oxidation, you may not be able to double reflow PCB. Can you do it in one cycle? One of the greatest challenges with bare copper PBCs is solder thieving from no solder mask. good luck Evamaria Jones Spec Tech -----Original Message----- >From: Ioan Tempea <[log in to unmask]> >Sent: Mar 19, 2008 8:42 AM >To: [log in to unmask] >Subject: [TN] Shelf lif of bare copper boards > >Dear Technos, > > > >Anybody using PCbs with bare copper pads and traces, no plating, no OSP, >not even solder mask? Because I have a few questions: > > > >What is their shelf life? > >Are they suited for double side SMT reflow? I mean, during the first >reflow the oxidizing is accelerated... > >What storing/handling procedures you use? > >Does the copper require any particular specifications, in order to >perform better in soldering? > >Anything else? > > > >Thank you, > > > >Ioan > > > > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 15.0 >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------