Hi Vector! Where is the 25% requirement in A610? I did not find a requirement listed for the thermal pad coverage. Dave Hillman Rockwell Collins [log in to unmask] Victor Hernandez <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 03/05/2008 07:49 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to [log in to unmask] To [log in to unmask] cc Subject [TN] QFN Thermal Plane Voiding Fellow TechNetters: The 25% solder voiding has been an accepted rule of thumb for QFN, Quad Flat w/No Leads, IPC-A-610D sec. 8.2.13. Is there any other guideline out there. Victor, --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------