Mornin' All! If the solder in a wave solder pot gets a little hot, it doesn't really degrade it does it? Situation is; I'm emptying three solder pots, one 63/37 pot, one SN96 pot, and one HMP pot, the way the pots are designed is that the pot thermocouples are located up towards the top of the pot. So as I lower the level of the solder in the pot, at some point the thermocouples will not be in direct contact with the solder and thus not be giving me the actual solder temperature. I've been cycling the heater power off when it looks like the solder is getting pretty hot (it starts getting getting this golden sheen to it), along with disconnecting the heaters when they start getting exposed as the solder level goes down. I've always emptied pots this way, and just started wondering if the solder degrades at all if you heat it up beyond the liquidous temperature. I know it makes a little more dross as the temperature rises... Steve --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------