Hi Ilkka - Since the root cause is still unclear, can you provide some information about the failure mode? For example: 1. What is the appearance of the solder pads in the missing component locations? Is there evidence the component was broken off (ie, a solder joint was formed and then fractured) or any indication of solderability issues (ie, the pads show de-wetting/non-wetting)? Keep in mind solderability problems could be due to component issues as well as PCB, but we examine the evidence we have. 2. If a component solderability issue is suspected, you might try tracing the failures to date codes, but with passives used in bulk that might be difficult. 3. What type and sequence of soldering processes are used? At what step are the missing components soldered? 4. Are the components normally glued when placed? Any evidence of problems? 5. Is missed placement a possibility? In other words, does the assembly equipment or downstream AOI (if used) detect a missed placement? An indication of this would be perfectly solderd pads without components. Missing is possible if the placement mechanisms are not properly adjusted, dirty or worn. I'm assuming they are placed with a high-speed chip shooter, vacuum suction force and timing may be an issue. Another possiblity is if the tape reels are mishandled before loading or by machine maslfunction. TGAsia has many experienced assembly engineers, if you provide more information, perhaps they can help. Regards, C.B. Katzko, CTO Meadville Group e-mail [log in to unmask] tel +86 21 3774 7528 fax +86 21 3774 7590 mobile +86 13817362590 +++ Please note new tel & fax numbers. +++ Ilkka Lehtinen <[log in to unmask]> 发件人: TGAsia <[log in to unmask]> 2008-01-11 16:54 请答复 给 [log in to unmask] 收件人 [log in to unmask] 抄送 主题 [TGA] SMD components cracking off Hi, I'm Mr. Ilkka Lehtinen, a Quality Manager in Teleste Corporation's (a Finnish company) manufacturing company in Suzhou, China. It's honor for me also to join this discussion forum. Our contract manufacturer has a problem they cannot solve themselves with SMD components: every now and then we find boards that have one or two SMD capacitors, resistors or inductors fallen off the board somewhere during the manufacturing process. The resistors and capacitors are 5-sided termination components and inductors are bottom only termination components. Normal stuff. The size is 0603. The problem is not location specific so it's not caused by some mishandling or that some areas are somehow prone to this kind of behavior. I'm out of glues. Has anybody faced this kind of problem or have any idea? Thanks in advance, Ilkka Lehtinen Quality Manager Teleste (Suzhou)