----- Original Message -----From: [log in to unmask] href="mailto:[log in to unmask]">huanan_6230To: [log in to unmask] href="mailto:[log in to unmask]">[log in to unmask]Sent: Thursday, January 10, 2008 2:04 PMSubject: [TGA] 双面贴装请教各位:双面纯贴装工艺的板子,是否必须过两次回流,前后用两种温度不同的焊膏呢,还是用一种焊膏直接过一次回流即可,这样是否会对焊接质量或元件本身造成损害?谢谢赐教!中国通号公司 张桦楠