From a solder paste and flux Product Development standpoint, EM was always tougher to pass then SIR. Part of reason being that the lower voltages used in EM would tend to preserve dendrites, whereas the higher voltages used in SIR would tend to blow them away. If you passed something like the Bellcore EM it was highly probable that you'd pass the IPC SIR test Rich Kraszewski / Kimball-GTS -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Schaefer Sent: Thursday, January 10, 2008 6:02 PM To: [log in to unmask] Subject: [TN] ECM or SIR - What Electrical test is best? Techneters, I am having to perform some tests to qualify the wash process using an alternative cleaning chemistry and would like to know what the real differences are between the ECM and SIR tests besides the time it takes to perform the test measurements. Thanks Much, Chris --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------