TechNetters, Coming back to my original question: are there specs out there for warpage at temperature (other than RT)? Here is what I have directly and indirectly from Graham Nasbitt. IEC 60191-6-19 Ed.1: Measurement methods of package warpage at elevated temperature and the maximum permissible warpage (This is a DRAFT document. It talks about shadow moiré and laser measurement of warpage. It also contains pass/fail criteria. In its current form it appears to be just an English translation of a Japanese document. I am compiling editorial comments to submit back to the IEC.) "High temperature package warpage measurement methodology", JESD22B-112, Aug. 2005. (Contains the shadow moiré method, but no pass/fail criteria.) Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, January 08, 2008 5:24 PM To: [log in to unmask] Subject: Re: [TN] SV: [TN] Warpage of components Hi Inge! I bet you're referring to Stablcor... http://www.stablcor.com/ At a past life the company that I worked for looked into the material to help ruggedize a Single-board Computer. Didn't really get to play around with it though. Couldn't get all involved to buy-off using the material because it was so new. But I must say, it looks pretty interesting! Wish I could have got some experience with it. Steve Gregory -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord Sent: Tuesday, January 08, 2008 3:16 PM To: [log in to unmask] Subject: [TN] SV: [TN] Warpage of components If someone has a 'warpage' problem, there is a way to design boards that are less apt to bending. NASA are working with new ideas, and Glenn Research Center together with Applied Materials, are making the new hardware. This is a carbon cloth, that is integrated with the FR4. The benefit is better cooling, better electrical performance and much stiffer board, the later means little or no warpage. I've seen these boards, but can't find the source at the moment. I'm sure someone on TN have more to show us here. If there are patent matters that hinder you for using the concept, I don't know. If I find more on this theme, I'll be back. /Inge -----Ursprungligt meddelande----- Från: Hfjord [mailto:[log in to unmask]] Skickat: den 8 januari 2008 16:56 Till: 'TechNet E-Mail Forum'; [log in to unmask] Ämne: SV: [TN] Warpage of components I promised a simple warpage calculation formula, if not too many, I'll send offline... Inge -----Ursprungligt meddelande----- Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier /* Skickat: den 8 januari 2008 14:15 Till: [log in to unmask] Ämne: Re: [TN] Warpage of components HI Ingemar, Well said. A warpage criterion for components would have to be based on a total out-of-plane measurement at soldering temperatures. This non-coplanarity measure would have to be about the thickness of the solder paste layer to avoid solder opens, and it would have to be based on the total final solder joint thickness to avoid solder joint cracking due to warpage tensile loads on cooling from reflow. Werner ************** Start the year off right. Easy ways to stay in shape. http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------