Hi Werner, I had HOPs in the past and the analysis was a warpage at the component corners that cause a delay in the soldering process (the flux was non active till the package was cooled back and the balls come back to the PCB pads). I used a special flux in the solder paste that have longer active time. I suggest to check if the BGAs have warpage during the reflow. Reuven e mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /* Sent: Friday, January 18, 2008 2:58 PM To: [log in to unmask] Subject: Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic Hi Bev, Just like George, I am struggling getting an understanding of you problem. To me, 'head-on-pillow' solder defects are almost always caused by insufficient peak temperature. If these HOP's occurred essentially near the center of the BGA, you have your answer, If the HOP's are distributed over the whole array, than the root cause is not insufficient peak temperature unless the whole reflow process is too low. Werner ************** Start the year off right. Easy ways to stay in shape. http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------