Phil, Here's the amendment to the RoHS Directive that covers your > 85% lead solder. See Page 2, Section 1. It adds this solder mix to the exemptions list. Dale Ritzen Quality Manager Austin Manufacturing Services -----Original Message----- From: Phil Nutting [mailto:[log in to unmask]] Sent: Thursday, January 17, 2008 10:17 AM To: [log in to unmask] Subject: [TN] hi-temp solder requirements Hi all, We have some applications where we have used Sn05Pb95 alloy solder that has a melting temperature of 301° - 314° C. Standard solders tend to melt when these devices go into a conduction mode and have a naturally high heat load that will of course "flow" down the component leads into the solder joint. Now that things are being converted to lead-free the question is being raised about this solder. So that prompts several questions. 1. I remember seeing somewhere in the RoHS specs a statement that >85% lead in a specific solder joint was an allowable exception. Is this true? I can't put my hand on the chapter and verse. 2. Is there a lead free alloy that is being used in industry that comes close to the melting temp of the Sn05Pb95 alloy? 3. Can some of this be solved by the pad shape and creating something that acts like a heat sink in the copper to dissipate the heat? 4. Has anybody else solved this problem? Thanks in advance. Phil Nutting Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------