Joyce, The gold is electroplated on the underbump metallization. I'm home and I left the thickness written on the board in the lab and I can't remember what it is right now. Bev ----- Original Message ----- From: Yuan-chia Joyce Koo <[log in to unmask]> To: TechNet E-Mail Forum <[log in to unmask]>; Bev Christian Sent: Wed Jan 16 19:36:38 2008 Subject: Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic where the gold come from? is it thicker than 0.1 micron plated form? Is it immersion gold or electroless? (the dissolution rate for plated/electroless/immersion are very different... not mention the organic complex exist on some of the surfaces)... jk On Jan 16, 2008, at 5:24 PM, Bev Christian wrote: > Dave, > I only have 0.8 to 1.2% gold in the solder balls - as determined by > XRF. > Bev > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman > Sent: Wednesday, January 16, 2008 5:06 PM > To: [log in to unmask] > Subject: Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold > Intermetallic > > Hi gang! Steve - I just sent you another set of photos showing a > solder > joint that has gold embrittlement. Bev - if you have a solder joint > that > contains the AuSn4 microstructure phase then you have an indication > that > your overall composition has exceeded the "magical" 4% limit. The > presence of the AuSn4 platelets cause the solder joint to behave in a > brittle manner when subjected to some use environments. The > formation of > the AuSn4 phase isn't going to interfere with the formation of your > solder > joint but they do result in solder joint integrity degradation. The > pretinning of gold plated component leads is an attempt to replace the > gold with a solder coating and lower the overall total percentage > of gold > that would exist in the solder joint - the lower the overall solder > joint > gold content, the lower the likelihood for the AuSn4 phase to form. > > Dave Hillman > Rockwell Collins > [log in to unmask] > > > > > Steve Gregory <[log in to unmask]> > Sent by: TechNet <[log in to unmask]> > 01/16/2008 03:35 PM > Please respond to > TechNet E-Mail Forum <[log in to unmask]>; Please respond to > Steve Gregory <[log in to unmask]> > > > To > [log in to unmask] > cc > > Subject > Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic > > > > > > > Hi Inge ol' pal! > > I went back and looked on my pages, and am not sure if they're still > there. But one of these might be: > > http://stevezeva.homestead.com/files/fracture_bad.jpg > > http://stevezeva.homestead.com/files/fracture_bad_2.jpg > > > Steve > > > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord > Sent: Wednesday, January 16, 2008 3:09 PM > To: [log in to unmask] > Subject: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold > Intermetallic > > Not really true, the Scottish blood in my veines tells me to be > careful > with money, the kyrgise blood makes me crush the table, therefore, > noone > can actually be under it. > > I think there are pictures from my large AuSn platelets somewhere on > Gregory's wall. If not, I can probably dig them up again from some old > report. If such crystals are abundant in a solder joint, the > components > may just jump off the board when giving a mechanical shock. > > /Inge > > -----Ursprungligt meddelande----- > Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier /* > Skickat: den 16 januari 2008 20:30 > Till: [log in to unmask] > Ämne: Re: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic > > Hi Inge, > As usual people are well advised not to argue with a (this) Swede; > 1) he > usually knows what he is talking about, and 2) if not, he will > drink you > under the table. > The IMCs formed by Sn/Pb, and Sn/Ag as well, are platellet-shaped > crystals > (in cross-section they may look like needles but are always > plateletts), > and I have seen no evidence that they are solderable. Solderability > simply > depends on how much Sn, or SnPb, to which you wet, is present. So the > amount of these IMCs affect both solderability as well as > Au/Ag-embrittlement. > Inge, how is Gerd? I sure have not heard anything about him for > some time. > > > > Werner > > > > ************** > Start the year off right. Easy ways to stay in shape. > > http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489 > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 To > unsubscribe, send a message to [log in to unmask] with following text > in the > BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or > (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE > mailing per > day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/ > archives > Please visit IPC web site http://www.ipc.org/contentpage.asp? > Pageid=4.3.16 > for additional information, or contact Keach Sasamori at > [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 To > unsubscribe, send a message to [log in to unmask] with following text > in the > BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or > (re-start) delivery of Technet send e-mail to [log in to unmask]: SET > Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the > posts: > send e-mail to [log in to unmask]: SET Technet Digest Search the > archives of > previous posts at: http://listserv.ipc.org/archives Please visit > IPC web > site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 > ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/ > archives > Please visit IPC web site http://www.ipc.org/contentpage.asp? > Pageid=4.3.16 > for additional information, or contact Keach Sasamori at > [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail > to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/ > archives > Please visit IPC web site http://www.ipc.org/contentpage.asp? > Pageid=4.3.16 for additional information, or contact Keach Sasamori > at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------------------------- > This transmission (including any attachments) may contain > confidential information, privileged material (including material > protected by the solicitor-client or other applicable privileges), > or constitute non-public information. Any use of this information > by anyone other than the intended recipient is prohibited. If you > have received this transmission in error, please immediately reply > to the sender and delete this information from your system. Use, > dissemination, distribution, or reproduction of this transmission > by unintended recipients is not authorized and may be unlawful. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail > to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/ > archives > Please visit IPC web site http://www.ipc.org/contentpage.asp? > Pageid=4.3.16 for additional information, or contact Keach Sasamori > at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------