It is OSP Panel feedthru connector made by MAACOM. Maacom has two options of the housing bushing plating : 1. stainless steel type 303 passivated per ASTM A 380 2. stainless steel type 303 with gold over nickel plating. Since option 1 is chipper we would like to purchase it, but our customer, who supposed to connect his mating connector, has connector made of stainless steel type 303 with gold over nickel plating. I hope it is clear now. Thank you in advance. Anat -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar Sent: Thursday, January 31, 2008 1:37 PM To: [log in to unmask] Subject: Re: [TN] galvanic compatibility this gives a different image. Seems like risk for galvanic currents. However, I'm still confused. A connector with passivated stainless steel 303?? What kind? And the gold plated connector, what's the body made of? Steel 303? Are you talking coaxial SMT SMA connectors or like? If that is the case, you must have steel-to-steel or gold-to-gold. /Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Anat Douek Sent: den 31 januari 2008 10:45 To: [log in to unmask] Subject: Re: [TN] galvanic compatibility Thank you for your response. It is not double plating. I have one connector with passivated stainless steel 303 and the mating connector is gold plating. The question is if it can be joined together, in high humidity level, without creation of corrosion Anat -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar Sent: Thursday, January 31, 2008 10:29 AM To: [log in to unmask] Subject: Re: [TN] galvanic compatibility Anat, why gold on passivated steel? Cosmetic aspect? Well, if it's a must, gold over steel is possible. There are lots of products with that finish, e.g. wrist watches. Passivation of steel is for protection against corrosion Gold plating is also for protection against corrosion. So, you want a double corrosion protection? Gold is not corrosive in itself and works as a corrosion protection if the gold is thick and free from pores. If too thin gold is used, corrosion can start through pores in the gold plating. So, if you happen to have minor contaminations in the steel AND a porous gold plating, there is a risk of pore corrosion. The steel surface roughness is also of importance. As always, there are some 'it depends'. If you describe the part to be plated, TN may give you a more precise answer. Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Anat Douek Sent: den 30 januari 2008 14:37 To: [log in to unmask] Subject: [TN] galvanic compatibility Hi, Is passivated stainless steel 303 can be joined to gold plating, in high humidity level, without creation of corrosion ? Regards, Anat --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------