Anat, The galvanic voltage should be about 0.5V. (0.25 claimed to be OK) It can be a big problem especially if the gold surface is bigger the SS. The SS will corrode eventually and the 303 is the fastest in the 300 series. With more salt in the water it will happen sooner. Ido Mashall www.beyond-materials.com -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Anat Douek Sent: Wednesday, January 30, 2008 3:37 PM To: [log in to unmask] Subject: [TN] galvanic compatibility Hi, Is passivated stainless steel 303 can be joined to gold plating, in high humidity level, without creation of corrosion ? Regards, Anat --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- -- No virus found in this incoming message. Checked by AVG Free Edition. Version: 7.5.516 / Virus Database: 269.19.16/1250 - Release Date: 29/01/2008 22:20 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------