Forgot to mention, a laser joint has a unique cooling profile. Solder joints formed by reflow techniques cool from the outside to the inside, as they cool generally by convection. Laser solder joints cool from the inside to the outside, as they cool by conduction of the heat in the joint into the surrounding materials that were not heated to the same temperature as part of the soldering operation. John Burke (408) 515 4992 -----Original Message----- From: John Burke [mailto:[log in to unmask]] Sent: Thursday, December 06, 2007 10:57 PM To: 'TechNet E-Mail Forum'; [log in to unmask] Subject: RE: [TN] Laser Soldering vs Selective Soldering You have to be very careful how you "melt it" too much power and you will "splatter" due to explosive flux heating. The beam movement is actually an art form, it is scanned as a lissajous figure over the surface of the joint so that the joint is evenly heated and the beam is not just "zapped" in one spot. It is indeed very cad dependent, but more than that it needs extensive R and D by the equipment OEM to ensure that typical beam movement profiles are available for a range of components. In the case of a BGA you can solder the device through the package using a YAG laser without overheating the surrounding area which is why such systems can be used for re-work. No they are not new. In 1987 we had a fully interfaced laser soldering system from Basel laser teknic of Starnberg in Munich, in exhibitions in the UK and Germany. These were fully featured systems working at full production speed (in those days not that fast actually) We had it connected from memory to a Siemens MS72 on the front end with an electrovert cleaner connected to the other end. John Burke (408) 515 4992 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz Sent: Thursday, December 06, 2007 5:00 PM To: [log in to unmask] Subject: Re: [TN] Laser Soldering vs Selective Soldering TechNet - I know our MacDermid booth was next to "BeamWorks" at the SMTAI show in Orlando in October. I just thought laser soldering by BeamWorks was a new idea. I have absolutely no opinion about BeamWorks except I got some ideas for special applications from seeing them work their laaser soldering machine. I can guess that laser soldering is quite CAD/Gerber programming dependent. Seems to me they were dispensing and laser soldering - guess if you know where you dispensed it, you know where to melt it. Comments? Denny Fritz MacDermid, Inc. In a message dated 12/6/2007 5:42:48 P.M. Eastern Standard Time, [log in to unmask] writes: Yes it did fade away, although I am not sure it ever really blommed. I remember when I put a laser soldering YAG system on the SMARTEX exhibition production line in Wiesbaden Germany in 1987 that : A It worked fantastically well B Everone was excited about it C The yields were fantastic D Nothing ever came of it...............cost?? **************************************Check out AOL's list of 2007's hottest products. (http://money.aol.com/special/hot-products-2007?NCID=aoltop00030000000001) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------