Thanks for the responses both on and off line. I put out the request because I was fed up with paying $8 for a small spray can of "gun degunker" For anyone interested if you mix 1 part of SLX denatured alcohol with 3 parts of deodorized mineral spirits (both at home depot), you will get the same result as a well known brand of gun cleaner - at less than one quarter the cost. Have a great Christmas all on Technet. Kind regards, John Burke "I asked Santa for a Turkey - he sent me lead free soldering" John Burke (408) 515 4992 -----Original Message----- From: Guy Ramsey [mailto:[log in to unmask]] Sent: Friday, December 21, 2007 10:48 AM To: 'TechNet E-Mail Forum'; 'John Burke' Subject: RE: [TN] Solvent Coleman cook stove white gas? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke Sent: Friday, December 21, 2007 12:22 PM To: [log in to unmask] Subject: [TN] Solvent Hi guys, I am looking for a "buy it at the home depot" solvent that will work the same as hexane. MY choices at home depot are MEK, Toluene, Acetone. Advice appreciated this is nothing to do with electronics!!!!! John John Burke (408) 515 4992 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------