I have seen what the Hinkle guy described in the referenced thread. The paste brick remains intact but something in the paste fails to encourage wetting of the individual spheres to each other and the component. I think it looks more like a lump of silver caviar. The condition is usually profile related. I have seen it induced by letting the paste dry prior to reflow. Most pastes have such long life now days that you only see it in a Designed Experiment. Perhaps new Pb-Free pastes are more susceptible. I have seen one instance attributable to solder paste failure. Soldering to a machined socket pin mounted on a very thick board with a validated profile results were poor (A lot of inspector whining). Noting that the paste was near the end of our permitted open life, we switched to a new jar and got good results. I suspect that even this was, to some extent profile related. We were operating on the long edge of the maximum "soak" time in a straight ramp to reflow because of the nature of the application. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Phillip Bavaro Sent: Thursday, December 13, 2007 6:06 AM To: [log in to unmask] Subject: [TN] "Grape-ing" My solderpaste supplier is educating me regarding a defect called "grape-ing". Anyone care to shed a little light on this soldering defect? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------