Good Morning Steve, We have 2 Electrovert Econopak's here that we purchased at Speedline Technologies. One is about 10 years old and the other about 2 years old. We use one for leaded solder and one for lead free. We have had very little problems with them and the tech support when we did have a problem was excellent. One has a foam fluxer and the other a spray fluxer and both have put off good quality product. Yes, we do have to do some touchup but don't think there is a machine out there that will give you zero defect off of it. Hope this helps in your selection. Regards, Bob Arciolla Endicott Research Group Quality/Safety Manager 607 754-9187 ex 3034 607 754-9255 fax cell 607 624-8516 ----- Original Message ----- From: "Steve Gregory" <[log in to unmask]> To: <[log in to unmask]> Sent: Thursday, December 06, 2007 8:26 AM Subject: [TN] Wave solder machine recommendations? Morning all! Just taking a quick poll, who would you recommend as far as wave solder machine manufacturers taking into account machine performance, machine quality, and customer support (not necessarily in that order). We're thinking about a new machine... Steve Gregory Production Engineer OAI Electronics 6960 East 12th Street Tulsa, Oklahoma 74112 (918) 836-9077 Ext 507 (918) 836-0184 FAX (918) 706-2779 Cell --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------