There are two things here, at least. Most low-temp (<500°C) couples use chromium-nickel and aluminium-nickel alloys. The precision depends on the accuracy of the alloys and it would be foolish to rely on new ones as better than ±2°C. Then, after time, there is a migration of intermetallics and this will reduce the accuracy further. This is more rapid at high temps (thanks, Mr Arrhenius!) and time/temp is more important than cycling. Thermocouples are never used for precision measurements at <250°C; platinum resistance thermometers (Pt100) are usually better than ±0.1°C, but their physical size and thermal inertia rules them out for profiling. With thermocouples, there is also the problem of cold junction compensation, which can further reduce the accuracy. For reference, although irrelevant here, only platinum (Pt/PtRh13) thermocouples are considered accurate to better than 1°C, provided the cold junction is in melting ice. Their downside is that they are very insensitive so are really useful only for high temperatures (>800°C). Brian Steve Gregory wrote: > Hi Everyone! > > How many reflow profiles do ya'll put the same thermocouples through > before you think about replacing them? > > I've typically used them until they quit working or the insulation > deteriorates so bad that I don't want to use them anymore. I was told > that was not a good practice. That your typical K thermocouple starts > drifting after only 4 or 5 thermal cycles. I said; "Really?" I didn't > want to debate a whole lot because it was a customer who said this, so I > just agreed and went on. > > So, do any of you know this to be a fact, and do any of you trash a > thermocouple after only 4 or 5 profiles and replace them with new ones? > > Kind regards, > > Steve Gregory > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------