Thanks Peer, so it's not the plating 8-{ Have to play a little bit more with the reflow, forgotten to mention the connector is SMT. Regards, Ioan -----Original Message----- From: P. Langeveld [mailto:[log in to unmask]] Sent: Friday, October 26, 2007 10:48 AM To: TechNet E-Mail Forum; Tempea, Ioan Subject: Re: [TN] Component pins plating thickness Ioan, The answer is 2-fold: 1. The measured finish layers are OK. The manufacturers spec however are, too lean. Already in the lead age the Ni-layer should be 0.002 mm (80 microin), the minimum Sn thickness 0.005 mm (200 microin). Otherwise the risk of the Sn layer is not hermetic sealing the Ni layer and the latter can be oxidized. And give wetting problems, and even more in PTH's. 2. I presume the connector is wave soldered at say, 265 dC. The (matte) tin has a melting point of 231 dC. Added with the thermal mass of the internal metal contact lips and other internal heat sinks in the board, the (total) contact time on the wave(s) has to be increased with about 1 second. Success. Peer Langeveld Consultant Soft Soldering Processes 5502 VH 8 The Netherlands 2007/10/26, Tempea, Ioan <[log in to unmask]>: > Hi Technos, > > I'm having a tough connector here, hard time to get all the pins soldered. > > It is matte Sn over Ni finished, measured coating thicknesses are 250 microinch Sn over 80 microinch Ni. Are these values OK? Isn't the Ni too thin and the Sn too thick? > > The manufacturer spec is 0.001mm (40 microin) minimum Sn over 0.0013 (51 microin) minimum Ni. > > Thanks for your input, > > Ioan > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------