Tom, Laser cutting openings with these spaces between is not an issue. Bill Kunkle MET Assocs -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Gervascio, Thomas Sent: Friday, October 19, 2007 2:18 PM To: [log in to unmask] Subject: [TN] Solder paste slump patterns Got a question, I was looking at the IPC-A-21 solder paste slump pattern and noticed that some of the spacings between pads were 0.05mm, .1 mm- this is .002" and 0.004"- and I can't imagine being able to etch a stencil with these spacings. Am I reading something wrong here? Any other newer solder paste slump patterns out there? Thanks Tom --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------