Brian, Inge and Rudy, It was recommended by a consultant for cleaning our mineral oil dielectric covered boards and assemblies. I had suspected is was on the "not desirable " list but wanted to confirm it. We have been having trouble with the quality of the oil. I strongly suspect it was the IPA used to submerge wash parts prior to assembly with a very short period of time to flash off the IPA. A dielectric test of the oil with 1% IPA added as a contaminant dropped the dielectric value by over 60%. Yikes! We are looking at a revision to our process. IPA is gone. I knew from previous posts that IPA was not the best product for cleaning. I just couldn't convince the curmudgeons who have been using it for 30+ years that it was giving them a false sense of security. Thanks for your wisdom. Maybe with this info I can keep heptane out of the process and facility better than the IPA. Phil -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis Sent: Friday, September 14, 2007 3:18 AM To: [log in to unmask] Subject: Re: [TN] Using heptane for cleaning For cleaning WHAT? Excellent degreaser but pretty hopeless for flux residues. I presume you mean n-heptane (there are several isomers). Flash point of ~-2°C and highly volatile. It requires a concentration of only about 1% in air to form an explosive mixture (it is possible that heptane was used as part of the aerosol mixture used in the new Russian "father of all bombs"). It is toxic and sufficiently persistent to be declared dangerous for the environment, especially in aqueous media. It has a whole host of risk and safety phrases under EU legislation. Not recommended. Brian Phil Nutting wrote: > Is anyone using heptane for cleaning? If so, what personal protection > systems have you put in place? > > Thanks in advance, > > Phil Nutting > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------