All,
 Got a question or two for the group. We have a situation where we are experiencing pads and traces being lifted during BGA removal. We use an Summit 1800 Machine and have verified calibration and thermal profiles  (even used an external device, ECD Mole to verify the profiles and temps). The products range in sizes as well as the BGAs. The surface finish is ENIG and the board venders are the same for all the products. Some of the products are Pb Free and others are standard lead products. 
 What types of testing can be done to verify tensile strength and copper adhesion? What other actions would you recommend?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------