I thought so. How could something like that be applied, as Bev correctly pointed out. There are too many variables that would determine the number of "safe" reworks. I prefer the term "Tg excursions" when a rework limit is set on agreement with customer and supplier. And a careful qualification is needed, as Bev pointed out, and it is usually a worthwhile effort to do so. Solder touchup and hand-soldering are usually excluded from this number, as this type of rework seldom leads to reliability issues. But again, there are exceptions. In addition to having "seen thin boards delaminated after a single, poor attempt at rework" I have also seen any given size and thickness and material type delaminated in spite of very careful qualification of the rework process. Also, I have seen Z-axis expansion as a result of too large of a delta T between the localized rework site and the rest of the assembly cause damage to vias and PTH barrels that went totally undetected by a careful inspection and X-ray and electrical test, including stress screening, only to fail later. This is why the hard limitation of the number of reworks was deleted when the standards changed from WS6536E, to J-STD-2000, to today's J-STD-001D and IPC-A-610D. There is no number of Tg excursions that is "safe" for every application. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian Sent: Tuesday, August 07, 2007 12:09 PM To: [log in to unmask] Subject: Re: [TN] Rework question Same here. Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke Sent: Tuesday, August 07, 2007 12:55 PM To: [log in to unmask] Subject: Re: [TN] Rework question Just looked in 7711 - didn't see a reference to it... John John Burke (408) 515 4992 -----Original Message----- From: Guy Ramsey [mailto:[log in to unmask]] Sent: Tuesday, August 07, 2007 9:14 AM To: 'TechNet E-Mail Forum'; 'John Burke' Subject: RE: [TN] Rework question I don't think it is worded as a hard limit. Might be IPC-7711. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke Sent: Tuesday, August 07, 2007 12:04 PM To: [log in to unmask] Subject: Re: [TN] Rework question The question actually came up because there is stated (somewhere?) in an IPC document the number of reflow cycles you are allowed to put the board through. Taking that limit into account (first side reflow, second side etc) allowed them to remove and replace the same component 3 times in a worst case scenario. And I agree with Bev the whole thing is open to interpretation as to what represents a reflow cycle - pad dressing removal etc. John Burke (408) 515 4992 -----Original Message----- From: Bev Christian [mailto:[log in to unmask]] Sent: Tuesday, August 07, 2007 8:53 AM To: TechNet E-Mail Forum; John Burke Subject: RE: [TN] Rework question John, I am having people look, but if there is a limit I do not remember. However, from a practical point of view, the answer is Doug Pauls' patented (Or is that copyrighted or trade marked? Being a lawyer, I don't know.) phrase, "It all depends". It depends on the method of rework, (reflow, wave solder, selective soldering, soldering iron, hot air gun focused IR, flame), temperatures reached, ramp rates, dwells, size of board, thickness of board, type of component, heat sinks, skill of operator. I could go on. Make yourself a fishbone diagram. And then are we talking about say 3X of the same component, or 5X side-by-side or 7x but each in a thermally separated area from the other six? Here's a scenario for you: double sided reflow and then required rework under cans on both sides of the board. So this means two more for can removal, dressing the can pads, removing the components, dressing the pads, part deposition, can replacement. And hope everything works! So you need visual inspection, x-ray inspection, electrical test and if you really want to do it right, x-sectioning and a whole battery of reliability testing. I have seen good work and I have seen thin boards delaminated after a single, poor attempt at rework. Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke Sent: Tuesday, August 07, 2007 10:29 AM To: [log in to unmask] Subject: [TN] Rework question Hi, I had a question yesterday which was "has the number of re-work cycles allowed by IPC changed for lead free?" And I confess I don't know but I bet someone on this link does. If you could let me know number of thermal cycles allowed and the spec reference I would be grateful. John John Burke (408) 515 4992 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------