Be sure that your air compressor and line are dry. They tend to fill-up quicker in humid times and may require more preventive maintenance. Sometimes a solvent switch to a different system helps; Rich K / KEG-GTS -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hogg, Blair K. Sent: Friday, July 27, 2007 2:49 PM To: [log in to unmask] Subject: [TN] Conformal Coat - Milky / Hazy appearance Technetters, We spray some of our conformally coated boards by hand and air dry them. The area used for this is not air conditioned and during humid times we sometimes see boards with a hazy appearance. Any thoughts on how we can correct this, other than air conditioning the spray booth? Thanks, Blair ******************************************************************* This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the system manager. This footnote also confirms that this email message has been swept for the presence of computer viruses. www.Hubbell.com - Hubbell Incorporated --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------