I have a quick question and our standard that we have maybe an older one. We currently use the ANSI/IPC-A-600 Rev E Page 70 Micro section: There is a table describing copper plating thickness min, requirements Class 1 Class 2 Class 3 Average Min Thickness .020mm (0.0008in) 0.025mm (0.001 in) 0.025 mm (0.001 in) Minimum this area .0015 mm( .0006 in) 0.020 mm (.0008 in) 0.020mm (.0008 in) Can anyone tell me if this still is a current standards for copper plating thickness measurements. David Harman --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------