Hello Noralee, This requirement is meant to assess the overall "indentations" on a surface in a 300mm x 300mm square area. The difficulty with analyzing several indentations of different sizes is that you cannot just count them (1, 2, 3) and make them equal as a larger indentation is a bigger issue than a smaller one. So the "point value" chart assigns bigger indentations a larger number than "1" as they can be a bigger issue. So if a CCL surface (300mm x 300mm) has 3 (0.18mm indentations) "point value of 1", 2 (0.36mm indentations) "point value of 2" and 1 (0.65mm indentation) "point value of 4", then the "point value" score for indentations is 11 (1+1+1+2+2+4). I now take that "point value" number of 11 down to table 3-4 "Surface Quality Classification" and see that with a point value of 11, my surface quality is "Class B". Please let me know if I or Microtek Laboratories can be of any further help. Best Regards, Bob Neves Chairman/CTO Microtek Laboratories Anaheim, CA +1 (714) 999-1616 Changzhou, China +86 (519) 548-7805 [log in to unmask] www.TheTestLab.com ________________________________ From: TGAsia [mailto:[log in to unmask]] On Behalf Of Li Yating Sent: Friday, June 22, 2007 1:28 PM To: [log in to unmask] Subject: [TGA] IPC 4101 comprehension Hi everybody, I have one question about IPC 4101 as the following. Could you tell me how to comprehend "Point Value"? Thanks a lot! Best Regards, Noralee Internet E-mail Confidentiality Disclaimer: This e-mail message may contain privileged or confidential information. If you are not the intended recipient, you may not disclose, use, disseminate, distribute, copy or rely upon this message or attachment in any way. If you received this e-mail in error, please return by forwarding the message and its attachments to the sender. Microtek Laboratories and its employees and agents do not accept liability for any errors, omissions, corruptions or virus in the contents of this message or any attachments.