Thank you Inge, this will help my company. My information is below: Paymon Sani, QE, P.Eng, M.A.Sc. Creation Technologies Inc. 110 Clegg Road, Markham, Ontario L6G 1E1 (905)754-5000, x5363 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar Sent: June 13, 2007 10:04 AM To: [log in to unmask] Subject: Re: [TN] Nickel barrier and RF applications Paymon Rockwell-Collins, Taconic, McDermid and HP investigated Nickel vs. RF. I can possiblysend the whole report to you offline. But first, whom are you working for? I'll ask Dave Hillman also, don't know if this report is official or not. Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani Sent: den 13 juni 2007 15:57 To: [log in to unmask] Subject: [TN] Nickel barrier and RF applications Hello John, is it documented anywhere? Paymon -----Original Message----- From: John Burke [mailto:[log in to unmask]] Sent: June 13, 2007 9:53 AM To: 'TechNet E-Mail Forum'; Paymon Sani Subject: RE: [TN] Plating The nickel in enig is not good for frequencies above 3 - 4 GHz John Burke (408) 515 4992 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani Sent: Wednesday, June 13, 2007 6:47 AM To: [log in to unmask] Subject: Re: [TN] Plating Hello Inge, This is very interesting! I did not make the connection between the Nickel on the PCBs and the RF application. Are there any papers that explain the sensitivity of RF applications to the Nickel barrier in ENIG PCBs? We are having trouble with a 5.8 GHz RF product right now. The assembly meets the IPC-610D requirement. However, 25% of the products fail testing. We reflow the failed assemblies for the 2nd time and 50% of them pass testing! We do not know the RC of the failures. I was suspecting the flux to be the root cause but could it be the Nickel barrier? Cheers, Paymon -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar Sent: June 13, 2007 2:33 AM To: [log in to unmask] Subject: Re: [TN] Plating Paul, Lockheed Martin use a lot of platings. I'm not sure, but I have seen Boron as a barrier somewhere, just can't find it right now. Anyway, Lockheed as well as NASA use many special platings. Non-magnetic, guess you have a RF application that need low-loss lines. http://supplier.external.lmco.com/supplier/po_information/specpro2.htm I was myself looking for a non-magnetic finish once, and if I remember right, there is a difference between EN and EN. The acidous electroless nickel is not ferromagnetic, while alcaline electroless nickel is somewhat ferromagnetic. Borohydride electroless Nickel-Boron is probably non-magnetic too. However, you should contact your plating chemist to verify, it was many years since I mixed with this. (In earlier days, we had our own chemists, many of them had piles of knowhow, but then came the economist's era, and the chemists were kicked out) Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stolar, Paul W Sent: den 12 juni 2007 23:38 To: [log in to unmask] Subject: [TN] Plating We are using nickel as a barrier metal on a PC board for the pads. Are there any other barrier metals we can use which are non-magnetic. Bare copper is not an option. Paul Stolar Materials/Reliability Engineer Manufacturing Reliability Lead Engineer Baker Atlas 713-625-5376 713-625-4949 (fax) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ------------------------------------------------------------------------ ---- ----------- Confidentiality Notice This e-mail and any attachment(s) are intended for the individual or entity to which this email is addressed and may contain information that is confidential. If you are not the intended recipient or an employee or agent responsible for delivering this e-mail to the intended recipient, please be aware that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this in error, please notify the sender by telephone at 604.430.4336 or by return e-mail, and please delete or destroy all copies of this communication. Thank you! --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ------------------------------------------------------------------------ --------------- Confidentiality Notice This e-mail and any attachment(s) are intended for the individual or entity to which this email is addressed and may contain information that is confidential. If you are not the intended recipient or an employee or agent responsible for delivering this e-mail to the intended recipient, please be aware that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this in error, please notify the sender by telephone at 604.430.4336 or by return e-mail, and please delete or destroy all copies of this communication. Thank you! --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------------------------- Confidentiality Notice This e-mail and any attachment(s) are intended for the individual or entity to which this email is addressed and may contain information that is confidential. If you are not the intended recipient or an employee or agent responsible for delivering this e-mail to the intended recipient, please be aware that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this in error, please notify the sender by telephone at 604.430.4336 or by return e-mail, and please delete or destroy all copies of this communication. Thank you! --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------