Dear Jim: IPC-A-610D Does not allow for class three for jumper wires to be inserted into a PTH which contains an existing lead. This is due to the potential CTE differences between the solder, jumper wire, lead and the barrel wall. Lots of different metals will likely cause a lot of stress in a Class 3 operating environment. Gregg Owens, MIT Manufacturing Technology Training Center, Inc. Mira Loma, CA 91752 -----Original Message----- >From: "Marsico, James" <[log in to unmask]> >Sent: Jun 8, 2007 11:12 AM >To: [log in to unmask] >Subject: [TN] ground wheels > >Hello Technet: > >Does anyone know of a requirement, industry or military, which prohibits >soldering 2 wires into one hole of a ground wheel? > >Thanks in advance, > >Jim Marsico > >EDO Corporation > >1500 New Horizons Blvd. > >North Amityville, NY 11701 > >631-630-5079 > >[log in to unmask] > > > > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 15.0 >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 >----------------------------------------------------- Gregg --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------