My employer is telling me that UL specifies the opperating tempature of the PCB material. From what I understand UL only specifies the flame rating and voltage rating. Proper opperating tempature is provided by the manufacture of the lamanate? Thats my question does UL specifiy the opperating tempature of the PCB lamanet? Here is what is stated on the old drawings. 1. CIRCUIT BOARDS MUST CONFORM TO UL 94 VERTICAL FLAME TEST AND UL796 2. MATERIAL: 0.062 +/- .006 THICK FR-4 LAMINATE - 2 LAYERS Here is what I have 2. Fabercate PCB in accordance to IPC-6012A Class 2; per IPC-6011 using the customer supplied data files. 3. Materials: A) Laminate and prepeg (B-stage) to be in accordance with IPC-4101/23 or IPC 4101/24. Material must meet UL 94V-0 Flammability rating with a Tg rating of 170 or greater is recommended. Finished thickness shall be .062 +/- .006 B) Copper foil to be in accordance with IPC-MF-150. Unless other wise specified, all copper weight for inner signal layers to be 35um (1 oz). For outer layers 71um (2 oz). Copper weight is to be considered "finished copper weight" I do not have a copy of UL 796 nor does my employer. I have no idea what that is or if thats where the temp rating comes from. I am pretty sure the guy is just cutting cost where ever he can and this is just one more place to cut them. I have just never heard of UL making recomendations for opperating tempatures of PCB lamate material. Thank you, Ted --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------