Hi Tom, Check the plating spec on the fab. The plating thickness in the via's should be specified at 0.001" absolute minimum if you are going with LF processes, regardless of the board material. (That is what I am told). I have made this change on my large 18+ layer boards, and my quality/yields have increased, and my opens have practically diappeared. Kerry McMullen Principal New Product Mfg. Engineer LTX Corporation 825 University Avenue Norwood, MA 02062-2643 (T) 781-467-5468 (C) 508-631-1832 (F) 781-461-0993 Tom Parkinson <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 06/05/2007 10:13 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Tom Parkinson <[log in to unmask]> To [log in to unmask] cc Subject [TN] Via Open Tech Net & Designer Net Greetings. We are running into a situation on Lead Free processed PCBs. Failure mode is finding open vias during unit testing (fully populated). Boards are Tg170, Material type EM320, 0.063" thick boards. 6 layers of 1 oz copper. ENIG 3~5u" Suspect vias go from top layer to bottom layer only. After running through reflow, we have found vias open. No visual signs of delamination, however when ohming out the via, if we press on the via we get continuity - thus we suspect the vias are opening during the process. Anyone out there having these problems, or information concerning this failure mode? Z-expansion failure? Tom Parkinson Quality System Manager - CIT WinTronics, Inc. Phone: 724-981-5770 - extension 235 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------