Emily and the Group,
I would like to expand on what Benjamin so
eloquently stated. In addition to what he stated below as reasoning for
the differentiation, UL also makes a distinction between inorganic filled and
unfilled CCL materials. It was the hope of the committee that UL would
use the designations of IPC-4101 specification sheets to define their “UL categories”
and this is another of the reasons for the separation into two specification
sheets.
I do agree with you that CTE will likely be
affected by the addition of inorganic material and that discussion is open for
the next revision of the slash sheet and document. In order to get the
specification sheets published in a timely manner, the committee left the
requirements the same between the filled and unfilled, but there is an
expectation that those requirements may change as more people participate on
the committee. Since you do feel strongly on this issue I would encourage
you to join the committee and comment and vote on this issue.
Best Regards,
Chairman/CTO
Microtek Laboratories
+1 (714) 999-1616
+86 (519) 548-7805
From: TGAsia [mailto:[log in to unmask]]
On Behalf Of Benjamin Chen
Sent: Tuesday, May 22, 2007 9:16
AM
To: [log in to unmask]
Subject: Re: [TGA] 关于IPC4101B中lead-free基材
Hi,
幸運地,我曾經參加過IPC-4101B的相關會議,敝公司也是訂定標準的公司,希望以下回覆能有些幫助!!
一般說來功能表是為了客戶使用上的方便與需要而存在,所以在大多數的情況下,為了考慮材料的多樣性與一般性,也讓客戶選料上的方便,同時也不希望功能表變成材料商的廣告,所以功能表上的功能會以該材料的平均性能列出,並不會列出極端的狀況。
同樣T'g但是填料與否的材料功能,雖然可能每一家製造商的狀況有所不同,但是平均而言,可能差異不足以到功能表更改所要求的差異。不過如果業界有普遍一致的證據與需求,依據我的經驗是可以向IPC提出更改的要求的。
Hope
this helps,
xxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxxx
Benjamin Chen
Regional Technical Coordinator, Asia-Pacific
Consulting and Training
Underwriters Laboratories Taiwan Co., Ltd.
Tel: 886-2-2896-7790 ext. 62267, Fax: 886-2-2896-6140
[log in to unmask]
- Know by test, and state the facts. -
Web site: http://www.UL.com.tw
emily luo
<[log in to unmask]> 05/22/2007 08:43 AM
|
|
大家好,
我想请教一个关于IPC4101B里lead-free基材的问题,IPC4101B中关于lead-free基材一共有六个产品性能表,Tg有110、150和170三种,每一种Tg又分有无机填料和不含无机填料两种,但同一Tg含或不含无机填料的产品性能要求却是一样的,我想这个是不是有些不太合理呢?如果性能要求一致,就没有必要分成两个产品性能表了,不知道大家对这个是怎么理解的呢?这样制定要求是否有什么特别的用意?
谢谢大家!
罗鹏辉
苏州生益科技
5-22
百万同时在线,人山人海同玩梦幻西游
- For more information about UL, its Marks, and its services for
EMC, quality registrations and product certifications for global
markets, please access our web sites at http://www.ul.com and
http://www.ul-asia.com or contact your local sales representative. --
********* Internet E-mail Confidentiality Disclaimer **********
This e-mail message may contain privileged or confidential
information. If you are not the intended recipient, you may not
disclose, use, disseminate, distribute, copy or rely upon this
message or attachment in any way. If you received this e-mail
message in error, please return by forwarding the message and
its attachments to the sender.
UL and its affiliates do not accept liability for any errors,
omissions, corruption or virus in the contents of this message
or any attachments.
*****************************************************************
Internet E-mail Confidentiality Disclaimer
This e-mail message may contain privileged or confidential information. If you are not the intended recipient, you may not disclose, use, disseminate, distribute, copy or rely upon this message or attachment in any way. If you received this e-mail in error, please return by forwarding the message and its attachments to the sender.
Microtek Laboratories and its employees and agents do not accept liability for any errors, omissions, corruptions or virus in the contents of this message or any attachments.