Hi Wayne, You should not "feel guilty about these ridiculous units, as a US citizen or otherwise." There are actually rather logical reasons (more than one) for these " ridiculous" "ounces per square foot" (1) copper is sold by weight, it does not matter whether you use ounces or kilograms; (2) unlike rolled copper, plated copper does not have a fixed density value— thus, there cannot be a direct conversion of "ounces per square foot" into mils ot kg/sq. meter into mm; (3) that has not stopped people from doing that, but they are ignoring a technical fact—which is really 'ridiculous.' (4) there is no real solution to this that would make everybody happy; (5) the interesting thing is that the laminators buy the ED foil by weight and sell it to you by area—guess what, all the laminated foil you buy is on the low thickness side of the spec. Werner ************************************** See what's free at http://www.aol.com. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------