Hi Sefika! Calculation seems easiest/fastest. You need to know what the weights of the copper are on each layer. The board was built with foils having specifications of "ounces per square foot" of copper (as a US citizen I do feel guilty about these ridiculous units!). Then plating will add a certain thickness. A decent "CAM" program, such as Pentalogix' "ViewMaster Plus" has a utility to calculate the area of the copper on each layer from the photoplots. Unless you have a very large ratio of vias to the area of the metal on each layer, you can ignore them. You could probably do a similar calculation knowing all of the data on the particular laminate selected, but the variance will be higher. Wayne Thayer >>> [log in to unmask] 5/22/2007 5:15:32 am >>> Hi, Is it possible to measure the mass percentage of copper of a pcb? Or, how can I calculate it theoretically? Do you have any experiance about this? Regards Sefika Dikkat : Bu elektronik posta mesaj* ki*iseldir. E*er, gönderilmesi gereken ki*i de*ilseniz lütfen göndericiyi bilgilendirip mesaj* siliniz. Firmam*za gelen ve giden mesajlar virüs taramas*ndan geçirilmekte, hukuki nedenlerle log kay*tlar* tutulmaktad*r. Mesajdaki görü*ler ve bak** aç*s* göndericiye ait olup Aselsan A.*. resmi görü*ü olmak zorunda de*ildir. Attention : This e-mail message is private. If you are not the intended recipient please delete the message and notify the sender. E-mails to and from the company are, monitored for virus protection and in accordance with lawful business practices. Any views or opinions presented are solely those of the author and do not necessarily represent the views of Aselsan A.S. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------