Telecordia and mil std still have the compliance requirements regarding the fongus. jk abcd -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Brian Ellis Sent: Tuesday, April 10, 2007 5:58 AM To: [log in to unmask] Subject: Re: [TN] Fongus treatment Fungicides used to be added to phenol-formaldehyde lacquers, in the days when all printed circuits were on cheap paper-based laminates (early 1950s, because the paper coating treater was poor in uniformity before stacking prior to pressing. However, that was also in the days when anode voltages were typically 250 V. I remember that 20 or so years ago, some conformal coatings contained fungostats and bacteriostats, but I haven't a clue whether they are still available. Normally, I would not expect modern materials to support mycelia penetration, so fungostats or fungicides should not be necessary. Beware that many fungicides are based on ionic metal salts! Brian Reuven Rokah wrote: > > One of our potential customer is interesting with "Fungus treatment" for > assemblies and cables. > > Do you familiar with such process? > > Thanks > > Reuven > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------