Werner: I have noticed that some of the FP ceramics components have very soft leads. Those leads will take all the mismatch from the two materials. The side problem with the soft leads is that they deform so easily. Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier Sent: Friday, March 16, 2007 11:08 AM To: [log in to unmask] Subject: Re: [TN] Engineering Question Well Kenny, Their concern may be CC racking, but could also be solder joint failures. Remember, there is a huge CTE-mismatch between the ceramic CC and the FR-4 PCB. Werner ************************************** AOL now offers free email to everyone. Find out more about what's free from AOL at http://www.aol.com. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------