I have seen this issue of voids due to the black hole process - excessive outgassing and poor solderability. Jeffrey Bush Director, Quality Assurance and Technical Support VERMONT CIRCUITS INCORPORATED 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302 Voice - 802.257.4571 ext 37 Fax - 802.257.0011 <http://www.vtcircuits.com/> -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of N Burtt Sent: Thursday, March 15, 2007 1:40 PM To: [log in to unmask] Subject: [TN] PCB laminate and immersion silver Anyone come across an issue when soldering through-hole/mixed tech PCBs using phenolic cured resin laminates, black hole plating process and immersion silver finish? This combination claimed to increase outgassing during wave solder (particularly lead-free solder) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------