Well Ramon, That is why they are called 'compliant leads'. They still store displacements elastically, thus the cyclic strain range is nbot reduced. however, the reason they work so well is that they drastically reduce the cyclic stress range, thereby reducing the area of the cyclic hysteresis loop which is a measure of the cyclic visco-plastyic strain energy which determines the cyclic damage done to the SJ. Whow--long sentence, but technically, if not grammatically, correct. So a QFP SJ is very reliable--very compliant leads, and a TSOP os not--very stiff leads. That's enough for a Friday. Werner ************************************** AOL now offers free email to everyone. Find out more about what's free from AOL at http://www.aol.com. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------