It is very common for 8-12 mil holes to have exposed copper where silver or even ENIG did not take because of soldermask residue not washed out of the holes. Are there clearances in the soldermask for these via holes. If there are not you could not begin to expect the hole walls to be covered with the silver finish. Gary At 08:57 AM 03/06/2007, you wrote: >Our customer is questioning what they feel is exposed copper in 8 mil vias >holes on silver boards. We feel there is mask residue in the holes >which does >not allow silver to take. These are holes that are allowed to be >plugged. Has >anyone else ran into this issue with thier customers and do you have the same >look or are your small vias covered with silver all the way through the via? > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 15.0 >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------