This is likely a case where the pads are being etched back as the sidewall of the inside pad/hole interface is copper and not tin plated. The basic "unwritten" rule for voiding is .005" maximum which will allow for adequate wetting to the hole/lead. A better process (and cheaper) is to use print and etch like an internal layer - this eliminates the voiding issue completely. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Skweres Sent: Thursday, February 22, 2007 11:41 AM To: [log in to unmask] Subject: [TN] "Fisheyes" Good morning. Does anyone know of any acceptability criteria for "fish eyes" or a thin void of copper around holes on single-sided boards? At times there's a complete cirmcumfrential void and other instances there's only a very small amount of copper missing. Thanks in advance for any assistance! Dan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------