James, You are right, there are 2 different finishes specified. One is immersion gold and the other fused tin-lead. This shouldn't make it past a board fab quotation though ... I'm sure they would contact you to confirm which one you need. Regards, Andre Demers, C.I.D. cmrsummit Technologies 329 March Road, Suite 203 Kanata, Ont Canada K2K 2E1 Telephone: 613.599.3881 Pager: 613.368.0506 Fax: 613.599.7889 -----Original Message----- From: DesignerCouncil [mailto:[log in to unmask]]On Behalf Of James Jackson Sent: Thursday, February 08, 2007 2:53 PM To: [log in to unmask] Subject: [DC] Contradictory Fab Notes? Okay folks, We have a client that we have contracted to fabricate a PCB for. They finally produced a Fab Drawing, and in the Notes, they have the following... 3.2 Board Material to comply with IPC 4101/21, FR4 Material. Copper Clad both sides, 1Oz Copper, 0.062 Thk, ENIG Plating finish. ... 3.9 Electro Solder Plate entire copper surfaces, .0003 minimum thickness and reflow solder (Infrared Fusing Preferred). .... Now... to my way of thinking, they have specified the PCB finish twice. In 3.2, they are wanting a gold finish (Electroless Nickel Immersion Gold). In 3.9, they are wanting a solder-plated finish. Or, am I mis-reading this? (I have left out the other notes 3.1, and 3.3 - 3.8, as they do not apply to this.) Could someone more knowledgeable set me straight? Regards, James Jackson Oztronics --------------------------------------------------------------------------------- DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF DesignerCouncil. To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF DesignerCouncil. To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ---------------------------------------------------------------------------------