Is there any silver content in the conductive ink? If below 100 ohms/sq then it probably has it intentionally and is a migration risk. There the risk of unintended silver in carbon ink as well. Long ago and far away i lived through an ugly humidity keypad field issue on a test deployment of wireless local loop phones in India. Finally discovered we were getting carbon ink that had residues of silver from previous mixes. You throw that silver into the mix with a phone operating with an continuously biased keypad, in a condensing monsoon environment in Bangalore, and voila! First failures came inside 30 days of fielding. Thank goodness for Bangalore traffic -- the test system installers were lucky to get around the city and install more than a couple phones/day. Most of the hardware was still on the shelf and we were able to recall and send reworked units to India and outfit a test system in Myanmar with properly reworked and re-qual'd units in the nick of time. The rework evolution and requal effort was a whole 'nother story involving walnut shells, lemon pledge and BB's -- takes at least 3 beers to tell it properly. Still have that qual plan around here somewhere... cheers, dw At 03:25 PM 12/15/2006, Carl VanWormer wrote: > > > > >The dielectric is Electordag 452SS UV Curable Dielectric Coating. The >manufacturer says they coat with 2 layers to reduce the chances of a >pinhole opening allowing a short circuit. Is this a possible clue of >something to chase for my humidity related shorts? > > >Carl Van Wormer >Cipher Systems >1800 NW 169th Place, Suite B-100 >Beaverton, OR 97006 >Phone (503)-617-7447 extension 20 > > > >-----Original Message----- >From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Lazzara >Sent: Thursday, December 14, 2006 6:08 AM >To: [log in to unmask] >Subject: Re: [TN] Membrane keypad failures > >In a message dated 12/13/2006 2:01:54 P.M. Eastern Standard Time, >[log in to unmask] writes: > >have two membrane keypads that have shown intermittent "short circuit" >failures. >Hello, Carl: > >OK, you've probably already looked for residual conductive ink between >conductors, but look closer for dust. Over-cured thick film >conductive polymers lose ductility and become [relatively] brittle. The >"...wiggling, banging..." >you described could produce enough conductive particulate between the >circuits to yield an intermittent high-resistance short. > >I'm also wondering about your dielectric: What is the dielectric material >(e.g., is it solder mask)? > > >ROBERT LAZZARA >VP, Business Development >T: (800) 560-9457 >F: (800) 878-5566 (y servicio de mensaje espaņol) >E: [log in to unmask] >W:_ www.CircuitConnectUSA.com_ (http://www.CircuitConnectUSA.com) > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e To >unsubscribe, send a message to [log in to unmask] with following text in the >BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or >(re-start) delivery of Technet send e-mail to [log in to unmask]: SET >Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: >send e-mail to [log in to unmask]: SET Technet Digest Search the archives of >previous posts at: http://listserv.ipc.org/archives Please visit IPC web >site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 >ext.2815 >----------------------------------------------------- > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------