It's a concern but easily addressed. I don't think the <1% reduction in lead usage arising from our going lead free will affect the availability of bismuth, nor do I think that any conceivable increased use of bismuth alloys in the electronics industry will do anything to overall bismuth usage. The amount of specialist alloys of all sorts used is small compared to mainstream solders, there would have to be a sustained geometric increase in rate of usage for this to be significant. Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of P. Langeveld Sent: Tuesday, December 12, 2006 10:40 AM To: [log in to unmask] Subject: Re: [TN] 58Bi/42Sn Another aspect on the use of Bismuth: Bismuth is a 3% by-product from lead-mining. Peer Langeveld Consultant Soft Soldering Processes. 2006/12/11, Kerry McMullen <[log in to unmask]>: > Hello esteemed Technet, > I am looking comments on what you would consider the advantages and > disadvantages of this composition of this solder paste. (58Bi/42Sn) > Lower MP. 138 Degrees C. > Lower fatigue resistance > Wetting to ImAg?? > Wetting to ImNiAu?? > No Clean? Residue? > Intermetallic Formation? > Mixing with 63/37Sn? > Our application is an RF board where we would use this paste post Wave / > Hand Solder. > Any comments appreciated. > > Cheers, > Kerry > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.*** --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------