Appears to be isolated/propagating from the SMT lands - possible touch-up issue? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of pearl petras Sent: Tuesday, November 28, 2006 11:59 AM To: [log in to unmask] Subject: Re: [TN] More delam This is standard FR4 with immersion silver finish. The standard soldermask colour we spec is clear, not green. Allows us to better see the copper, and often some inner layer features as well, but if you aren't used to working with FR4 with clear soldermask, it can definitely look a little strange, at first. The dark colour seen is due to an inner layer that is primarily ground plane. I'm pretty sure that it isn't soldermask bubbling We have not yet done any microsectioning. So far we have only seen this on fully populated boards that have experienced some hand-soldering, and we are reluctant to sacrifice one, if it can be saved for production. I have a blank two-up panel available from each manufacturer we've used. We are planning to run some hand-soldering tests. Vary temperatures, one unbaked and one baked from each panel, etc. Any other ideas? --------------------------------- All new Yahoo! Mail - --------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Get a sneak peak at messages with a handy reading pane. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------