Tom, Most people that I talk to do not use the same stencil. How clean is clean? If you are using an automated cleaning machine, the contaminants from the leaded can get into the Pb free stencil. Also, depending on the paste you are using, the Pb Free stencil may be made 1:1 solder pads to your board while the stencil for tin/lead may have reductions (the tin/lead solder alloys tend to have better wetting than most Pb free alloys). Kathy Jenczewski MicroScreen At 12:22 PM 11/30/2006 -0500, you wrote: >Hello all, > >SMT Stencils - Can we use the same stencil that was used for leaded paste, >for no-lead paste if they are properly cleaned? What's your thoughts on >this? > >Thanks > >Tom Parkinson >Quality System Manager - CIT >WinTronics, Inc. >Phone: 724-981-5770 - extension 235 > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------