Dear Technetters ... thank you all for sharing. I am very familiar with the different tests, how they work, what they test, when I might want to use one over another one ... what I was trying to do was follow a thread. Werner, I have read your paper and you say "The glass transition temperature should be determined using the Thermo-Mechanical Analysis (TMA) method as per IPC-TM-650, 2.4.24c. The TMA method is preferred ..." Also, Cameron Murray wrote in his Technical Paper, published by the IPC, and presented at IPC Printed Circuits Expo 1998, titled: Testing and Evaluation of HDIS Materials: "The IPC4104 committee has decided the preferred method for determining CTE and Tg is by use of a thermal mechanical analyzer (TMA)." So, I was only trying to find out if there was an official position or white paper from the IPC or an IPC committee. I have been specifying TMA for Tg for 20 years ... there are a few on this forum who go back with me to the old Digital Equipment Corp days, and way back then when we broke into 10 layer boards! that were .093 thick! we did an extensive round robin study of the 3 methods then correlated findings with 3 independent commercial labs ... so, you don't need to sell me. I was just looking to see, based on some people using the letters TMA close to the words IPC and "preferred", if there was a direct link. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Following Werner's response I conclude that there isn't ....