Steve, Is the oven running N2 or air? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 31, 2006 8:20 AM To: [log in to unmask] Subject: Re: [TN] Bizzare Phenomena... Victor, I didn't get out a set of calipers to measure the size of the solderballs...why would I need to do that? You can get a pretty good idea of how big they are in relation to the mesh chain of the conveyer and the screen covering the blowers. No, there aren't any components attached as you can see in the photos...just solderballs. -Steve Gregory- -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez Sent: Tuesday, October 31, 2006 9:08 AM To: [log in to unmask] Subject: Re: [TN] Bizzare Phenomena... When was the last time the reflow oven was cleaned? What is the size/diameter of the solder balls? Is this solder are components attached? Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 31, 2006 8:57 AM To: [log in to unmask] Subject: [TN] Bizzare Phenomena... Mornin' All! This morning I have seen something that I have never, ever have seen before. It's been a little slow the past week, so we decided to do our maintenance on our reflow ovens. After we opened the oven up, we found many, many solderballs laying on the bottom of the oven right around zone 7 - 8, right at the beginning of the spike zone. Check-out: http://stevezeva.homestead.com/files/Oven_Solderballs.jpg http://stevezeva.homestead.com/files/Oven_Solderballs_2.jpg http://stevezeva.homestead.com/files/Oven_Solderballs_3.jpg http://stevezeva.homestead.com/files/Oven_Solderballs_4.jpg We've been having tombstoning problems when we've run the two lead-free jobs that we have here. I've been working with the paste vendor sending my profiles and plots, but I haven't been able to solve the problem. The solderballs in the oven are lead-free solderballs. We are using a Heller 1809, and my profile set-points are: 120 140 160 180 190 200 230 240 250 120 140 160 180 190 200 230 240 250 Belt speed 26 in per min The paste is a SAC 305 with a water washable no-clean flux. I think my profile is pretty reasonable, and the last board we ran is pretty standard, .062" thick, with no bizzare copper planes. The board finish with both jobs has been ENIG. The last job I ran we were tombstoning 0805's, the one before that we were tombstoning 0402's. With both jobs we've had major tombstoning problems. I've slowed the beltspeed down, sped it up, ramped up slower, ramped up faster, changed this, changed that, but still haven't resolved my tombstoning. Of course, I'm the only one that's having this problem according to my paste vendor... I wouldn't have imagined that I would see the solderballs in the oven like we have... Have any of you ever seen something like this before? -Steve Gregory- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- This message (including any attachments) contains confidential and/or proprietary information intended only for the addressee. Any unauthorized disclosure, copying, distribution or reliance on the contents of this information is strictly prohibited and may constitute a violation of law. If you are not the intended recipient, please notify the sender immediately by responding to this e-mail, and delete the message from your system. If you have any questions about this e-mail please notify the sender immediately. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------