CTE for FR4 is only around 7 below the Tg. Get above the Tg and it rises to around 13/14 on both the x and y axis. Ceramic will stay at around the low figure throughout the whole thermal excursion. Z axis, however, will go from 50/70 to around 270/290 above Tg. This may or may not have an effect of the cracking effect dependant on pad design and area attached. Colin W.T. McVean M.Inst.C.T Production Manager Artetch Circuits Ltd Direct Dial 01903 712926 Switch Board 01903 725365 www.artetch.co.uk -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Neifer, Gebhard Sent: 19 October 2006 16:20 To: [log in to unmask] Subject: [TN] AW: [TN] Tombstoning and nitrogen Richard, my understanding is that ceramic chip capacitors are very sensitive to bending and tensile stresses, not to compressive loads. Since the CTE of such a chip component is 9 ... 12 [ppm/K] and the CTE for FR4 is 17 ... 18 [ppm/K] I do not really understand why cracks should occur during cooling after reflow. Can you please explain, thanks, Gebhard -----Ursprüngliche Nachricht----- Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Stadem, Richard D. Gesendet: Donnerstag, 19. Oktober 2006 16:44 An: [log in to unmask] Betreff: Re: [TN] Tombstoning and nitrogen Yes, Two different companies called me in the past few weeks where they were seeing an increase in MLCCC chip caps cracking. The first one had the problem with a new design, but they did not associate it with the fact that the process had changed simultaneously to a Pb-free process. The second company, they simply changed an existing power supply design over to a Pb-free process. They thought it was a fault of their board layout, but I explained to them that with the hotter reflow temperatures there is a longer cooldown from solidus to room temperature. Once at solidus the caps are locked in. But as the board continues to cool it imparts a major stress. Being that ceramic caps often have a much different CTE than the new pwb materials, they crack. The cracks are sometimes visible under 100X magnification, but are present immediately after reflow. They may fail electrical test immediately, or they will fail later. In both cases the same exact lots of capacitors did not exhibit this problem with standard 63/37 reflow profiles on other pwbs that (I suspect) are more forgiving. I had not thought of the lesser elasticity in the SAC alloy until you mentioned it, but all of these things work together. The more I see of the reliability issues related to Pb-free, the more it is impressed upon me that all of these failures are seldom the result of a single root cause, but rather a combination of different factors. So, another fallout from RoHS. ________________________________ From: [log in to unmask] [mailto:[log in to unmask]] Sent: Thursday, October 19, 2006 8:58 AM To: Stadem, Richard D.; [log in to unmask] Subject: Re: [TN] Tombstoning and nitrogen Hi Richard, You are absolutely correct. Large fillets also cause chip cracking, particularly with the stiffer LF-solders. Werner --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- **************************************************************************************** Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you. **************************************************************************************** --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------